In sunlight, there are stripe pigments in the products.
2018-06-28

Physical and mechanical properties of plastics:

1. The temperature of the injection molding equipment is not controlled well, and the masterbatch cannot mix well with the resin after entering the mixing chamber.

2, the injection molding machine does not add a certain back pressure, the mixing effect of the screw is not good.

3, masterbatch dispersion is not good or poor resin plasticization.

Process can be debugged as follows:

1. Increase the temperature of the mixing chamber slightly by the part of the blanking mouth

2. Apply a certain back pressure to the injection molding machine. If the above adjustment is still not good, it may be the problem of dispersibility or matching of masterbatch and resin, and contact the masterbatch manufacturer to solve it.

CONTACT US
contact us
Phone: 020-82253210, 82253219
Mailbox: bosi@vip.163.com
Address: No. 7, Yun Qing Road, Luogang District, Guangzhou, Guangdong

Sweep
Pay attention to the WeChat public number

Copyright©2013 Guangdong Persian Polytron Technologies Inc, Guangdong ICP 13064142-1Powered by Vancheer
Click here to send me a message